METAL
TREATMENT
High conductivity copper
Melt under reducing cover of copper cleaner E. C. powder Degas with T-Logas
Deoxidies by plunging De-oxidising tube.
C.B. (Containing Calcium Boride)
Commercial Copper
Melt under reducing cover of copper-cleaner powder. Degas with T - Logas. Deoxidize with De-oxidising tube 193 (containing phosphorus)
Tin-Bronze
Melt charge on top of Cleanex Block B briquettes in bottom of crucible or under a cover of copper cleaner standard powder. Degass with T. Logas. Deoxidies with De-oxidising tube 193.
Leaded Tin Bronze
Melt charge on top of Cleanex Block B in bottom of crucible or under a cover of Coppercleaner standard powder. Degass with T. Logas . 100 Deoxidise with De-oxidising tube 193.
Gun Metal and Leaded GunMetal
Melt charge on top of cleanex Block B in bottom of crucible or under a cover of Copper-cleaner standard powder. Degas with T. Logas, plunge De-oxidising tube 193.
Phosphor Bronze
Melt charge top of cleanex block 20 or under a cover of coppercleaner 20 powder. Degas with T. Logas. Plunge De-oxidising tube 193.
Brass and Leaded Brass
Melt under a fluid cover of Metalcleaner 49. Plunge de-oxidising tube 193 just before pouring.
Copper-Nickel Alloys (Nickel Solders and nickel Bronze containing 12-25%) (Ni) and Monel Metal.
Melt charge on top of cleanex block B or under a cover of Coppercleaner standard powder. Degass with T. Logas. Plunge De-oxidising tube Mg-6.
Brass and Leaded Brass
Melt under a fluid cover of metalcleaner 49. plunge de-oxidising tube 193 just before pouring.
Tin Bronze
Melt charge on top of cleanex block B briquettes in bottom of crucible or under a cover of coppercleaner standard powder. Degass with T. Logas Deoxidise with De-oxidising tube 193.
Leaded Tin Bronze
elt charge on top of Cleanex Block Bin Bottom of Crucible Or Under a cover of Coppercleaner Standard Powder, Degass with T. Logas 100 Deoxidise with De-oxidising tube 193.
Gun Metal and leaded Gun Metal
Melt charge on top of cleanex block B in bottom of crucible or under a cover of copper-cleaner standard powder. Degas with T. Logas. Plunge De-oxidising tube 193.
Phosphor Bronze
Melt charge on top of cleanex block 20 or under a cover of coppercleaner 20 powder a cover of copper cleaner 20 powder. Degas with T.logas, Plunge De-oxidising tube 193.
Copper-Nickel alloys (Nickel Solders and Nickel Bronze Containing 12-25% (Ni) and Monel Metal.
Melt charge on top of Cleanex Block B or under a cover of Coppercleaner standard powder. Degass with T. Logas Plunge De-oxidising tube Mg-6.
Brass and Leaded Brass
Melt under a fluid cover of Metalcleaner 49 plunge de-oxidising tube 193 just before pouring
Aluminum Bronze
Melt under a fluid cover of Albrol. No sooner pouring temperature is reached plunge small quantities of Albrol. Degas with T -Logas. Plunge E3 Tubes (Boron Manganese) before pouring.
Manganese Bronze
Melt under a fluid cover of Albrol. No sooner pouring temperature is reached plunge small quantities of Albrol. Degas with T -Logas. Plunge E3 Tubes (Boron Manganese ) before pouring.
Silicon Bronze
Melt under a fluid cover of albrol. No sooner pouring temperature is reached plunge small quantities of Albrol. Degas with T-logas. Plunge Deoxidising tube E3 & 193 tube before pouring.
Commercial Gun metal and Brass
Melt under cover of Metal Cleaner powder or Cleanex Block A. plunge Deoxidising tube 131 before pouring